Skip to content

Dyeing & Finishing: Special processes

Processes outside normal dyeing: mercerising knit fabric, stripping a faulty shade, and optical brightening for whites.

10 guides
Special processes

Heat setting of polyester and elastane knit fabric: how it works

Heat setting fixes polyester, nylon and elastane fabric at a chosen width at about 180–200°C. Typical settings, pre-setting versus post-setting, which knits…

Updated Oct 2026 6 min read
Special processes

Grey mélange fabric overdyeing process: soda scour, 80°C migration and the full reactive curve

Grey mélange overdyeing process for knit fabric: low-alkali soda and peroxide scour, reactive curve with 80°C migration, and running shade control.

Updated Oct 2026 2 min read
Special processes

Cationic dyeable (CD) polyester dyeing process: cationic dyes at 110°C

CD polyester dyeing process for knit fabric: acid pre-wash, cationic dyes at pH 4 and 110°C, blends with polyester and cotton, and…

Updated Oct 2026 2 min read
Special processes

Yarn-dyed knit fabric enzyme wash process: clean surface without colour bleeding

Yarn-dyed knit fabric enzyme wash: anti back-staining wash, enzyme at pH 4.5, hairiness check, fixing and softener, and how to stop stripe…

Updated Oct 2026 2 min read
Special processes

Natural dyeing process for cotton knit fabric: salt first, colour at 30°C, fix at 80°C

Natural dyeing process for cotton and organic cotton knit fabric: mordant, salt first, colour at 30°C, 80°C exhaustion, and fastness limits.

Updated Oct 2026 2 min read
Special processes

Antimicrobial finish on knit fabric: how we apply it in the dyeing machine

Antimicrobial finish on knit fabric: exhaust in the dyeing machine at pH 5–5.5 and 40°C, or padding on the stenter, and testing…

Updated Oct 2026 1 min read
Special processes

Fake mercerised (mercerise-look) knit fabric: getting the shine and crisp hand without mercerising

How to get a mercerised look on knit fabric without mercerising: singeing, hot alkaline loading, enzyme, and fixing without softener for a…

Updated Oct 2026 2 min read
Special processes

Stripping reactive-dyed cotton knit fabric: the process to remove an uneven shade

How uneven reactive-dyed cotton knits are stripped on a working dye house floor: the 98°C stripping bath, a reducing bath adjusted by…

Updated Oct 2026 4 min read
Special processes

Mercerised knit fabric dyeing process: gentle pretreatment, no enzyme, salt at 80°C

How mercerised cotton knits are pretreated and reactive dyed on a working dye house floor: a gentle 95°C scour, no enzyme, and…

Updated Oct 2026 4 min read
Special processes

Nylon white process: scouring, reductive clearing and optical brightening

How white nylon is made on a working dye house floor: soda scour, a reducing bath with the optical brightener at 98°C…

Updated Oct 2026 4 min read